Polyester-based Thermoplastic Polyurethane
| Properties | Key | NORM | Value | Unit |
|---|---|---|---|---|
| Hardness (after 3 sec.) | M | ISO 48-4 | 70 | Shore A |
| Hardness (after 3 sec.) | M | ISO 48-4 | 22 | Shore D |
| Density | M | ISO 1183-1 | 1.18 | g/cm³ |
| Tensile strength | M | DIN 53504 | 15 | MPa |
| Elongation @ break | M | DIN 53504 | 800 | % |
| Tensile stress @ 100% elongation | M | DIN 53504 | 2.2 | MPa |
| Tensile stress @ 300% elongation | M | DIN 53504 | 4.2 | MPa |
| Softening range low | E | Huntsman TMA | 95 | °C |
| Softening range high | E | Huntsman TMA | 115 | °C |
M = Injection molded parts to meet DIN & ASTM requirements. Parts at room temperature aged prior to testing.
E = Extruded film cut to ASTM requirements. Parts at room temperature aged prior to testing.