Polyester-based Thermoplastic Polyurethane
| Properties | Key | NORM | Value | Unit |
|---|---|---|---|---|
| Hardness (after 3 sec.) | M | ASTM D 2240 | 60 | Shore A |
| Tensile strength | E | ASTM D 412 | 4401 | psi |
| Elongation @ break | E | ASTM D 412 | 655 | % |
| Tensile stress @ 100% elongation | E | ASTM D 412 | 416 | psi |
| Tensile stress @ 300% elongation | E | ASTM D 412 | 700 | psi |
| Tensile set @ 200% Elongation | E | ASTM D 412 | 15 | % |
| Tear strength | E | ASTM D 624 | 308 | pli |
| Softening range low | E | Huntsman TMA | 105 | °C |
| Softening range high | E | Huntsman TMA | 135 | °C |
| Glass transition temperature (DSC) | E | ASTM D 3418 | -36 | °C |
M = Injection molded parts to meet DIN & ASTM requirements. Parts at room temperature aged prior to testing.