Polyether-based Thermoplastic Polyurethane
| Properties | Key | NORM | Value | Unit |
|---|---|---|---|---|
| Hardness (after 3 sec.) | M | ASTM D 2240 | 88 | Shore A |
| Hardness (after 3 sec.) | M | ASTM D 2240 | 42 | Shore D |
| Density | M | ASTM D 792 | 1.12 | g/cm³ |
| Tensile strength | E | ASTM D 412 | 8065 | psi |
| Elongation @ break | E | ASTM D 412 | 530 | % |
| Tensile stress @ 100% elongation | E | ASTM D 412 | 960 | psi |
| Tensile stress @ 300% elongation | E | ASTM D 412 | 1900 | psi |
| Tear strength | E | ASTM D 624 | 480 | pli |
| Abrasion | M | ISO 4649 | 28 | mm³ |
| Compression set at 22h @ 23°C | M | ASTM D 395 | 30 | % |
| Compression set at 22h @ 70°C | M | ASTM D 395 | 80 | % |
| Softening range low | E | Huntsman TMA | 160 | °C |
| Softening range high | E | Huntsman TMA | 170 | °C |
| Glass transition temperature (DSC) | E | ASTM D 3418 | -37 | °C |
M = Injection molded parts to meet DIN & ASTM requirements. Parts at room temperature aged prior to testing.
E = Extruded film cut to ASTM requirements. Parts at room temperature aged prior to testing.