Polyester-based Thermoplastic Polyurethane
| Properties | Key | NORM | Value | Unit |
|---|---|---|---|---|
| Hardness (after 3 sec.) | M | ISO 7619 | 90 | Shore A |
| Hardness (after 3 sec.) | M | ISO 7619 | 42 | Shore D |
| Density | M | ISO 1183-1 | 1,21 | g/cm³ |
| Tensile strength | M | DIN 53504 | 47 | MPa |
| Elongation @ break | M | DIN 53504 | 500 | % |
| Abrasion | M | ISO 4649 | 40 | mm³ |
M = Injection molded parts to meet DIN & ASTM requirements. Parts tempered for 20 hrs @ 100 °C prior to testing
Processing Parameter: Injection Molding
| Temperature Profile | °C |
| Feed Zone: | 25 - 40 |
| Barrel: | 195 - 220 |
| Nozzle: | 205 - 215 |
| Mold: | 20 - 50 |